Mechanical fatigue — symptoms, diagnosis and prevention
Cyclic stresses initiate and propagate cracks even below static strength.

What it is and how it occurs
Cyclic stresses initiate and propagate cracks even below static strength.
Typical symptoms and indications
Localized origin, possible propagation zone and final fracture.
How to investigate and differentiate
Fractography, cycle history, stress concentration and material.
Prevention and interventions to assess
Reduce stress concentrators, validate loads and inspect critical areas.
How to use in an investigation
Record the observed symptom, operating conditions and affected component. Add this record as a hypothesis; document supporting and opposing evidence and a test that distinguishes it from alternatives. Propose definitive actions only after validating the causal link.
Related equipment
Other mechanisms for comparison
Ductile fracturePlastic deformation and void coalescence precede fracture.→Brittle fractureA crack propagates rapidly with limited macroscopic plastic deformation.→Uniform corrosionChemical or electrochemical reactions reduce thickness broadly.→Pitting corrosionLocalized attack forms cavities that may penetrate the section.→
Supporting references
- ISO 17359:2018 — Condition monitoring and diagnostics of machines
Educational support. Actual investigations require evidence, risk assessment, applicable criteria and validation by responsible professionals. References do not imply standards compliance.
Turn knowledge into investigation
Use the methods in the software, organize evidence and export a report. Free, no sign-up.